METHOD FOR FORMING RUSTPROOF FILM ON PC STRAND
ກ່ຽວກັບ ສິດທິບັດ «METHOD FOR FORMING RUSTPROOF FILM ON PC STRAND» ໃນລາວ, ຍື່ນໂດຍ KUROSAWA CONSTRUCTION CO., LTD ໃນວັນທີ 2013-09-11; ສະຖານະ ປະຖິ້ມ. ຕົວລະບຸ: ເລກທີຄຳຮ້ອງ P/278; ລະຫັດ DIP LAP278; ປະເພດການປົກປ້ອງ Patent - Foreign. ວັນທີສຳຄັນ: ວັນເຜີຍແຜ່ 2026-01-16. ປະເພດ/ຫ້ອງ: B05D 3/02、B05D 5/00、B05D 7/20、B05D 7/24、D07B 1/16. ນັກປະດິດ/ນັກອອກແບບ: Kei HIRAI, Ryohei KUROSAWA. ສະຫຼຸບ: Provided is a method for the highly efficient formation of a uniform, high-quality film with which increased line speed, improved productiv…. ຂໍ້ມູນເພື່ອອ້າງອີງເທົ່ານັ້ນ ບໍ່ແມ່ນຄຳແນະນຳທາງກົດໝາຍ ຫຼື ໃບຢັ້ງຢືນສິດ.
P/278
ຮູບໝາຍ
ຂໍ້ມູນພື້ນຖານ
- ປະເພດ
- ສິດທິບັດ
- ເລກຄຳຮ້ອງ
P/278- ສະຖານະ
- ປະຖິ້ມ
- ຜູ້ຮ້ອງຂໍ
- KUROSAWA CONSTRUCTION CO., LTD
- ຕົວແທນ
- LAO Interconsult Co., Ltd
- ວັນຍື່ນ
- 2013-09-11
- ວັນເຜີຍແຜ່
- 2026-01-16
- ປະເພດການປົກປ້ອງ
- Patent - Foreign
- ທີ່ຢູ່ຜູ້ຍື່ນ
- KUROSAWA CONSTRUCTION CO., LTD · 1-26-7, Wakaba-cho, Chofu-shi, Tokyo, 182-003 Japan · JP
- ທີ່ຢູ່ຕົວແທນ
- LAO Interconsult Co., Ltd · Ban Sphanthong Tai, Sokpaluang Road P.O.Box 7039, Vientiane Capital, Lao PDR · LA
- ປະເພດສາກົນ
- B05D 3/02 · B05D 5/00 · B05D 7/20 · B05D 7/24 · D07B 1/16
- ສິນຄ້າ / ບໍລິການ
- —
ຂັ້ນຕອນ
ໝາຍຕາມສະຖານະປັດຈຸບັນ-
ຍື່ນຄຳຮ້ອງ
-
ກວດຮູບແບບ ບໍ່ຜ່ານ / ຢຸດ
-
ກວດເນື້ອໃນ
-
ເຜີຍແຜ່
-
ອະນຸຍາດ
ການວິເຄາະກ່ຽວຂ້ອງ
ເຊື່ອມກັບຖານຂໍ້ມູນວິສາຫະກິດ LaoBiz.comສິດທິບັດທີ່ຄ້າຍກັນ
ສະຫລຸບ
Provided is a method for the highly efficient formation of a uniform, high-quality film with which increased line speed, improved productivity, and cost reduction can be envisaged. A method for forming a rustproof film on PC stranded (1) conveying the PC strand through a process line, including untwisting step of untwisting the PC strand to separate surrounding wires (1b) from a core wire (1a) in the PC strand; a coating step of applying a synthetic resin powder coating material on each outer peripheral surface of the core wire and the surrounding wires in the untwisted state; a heating step of heating to adhere the coating uniformly on the core wire and the surrounding wires; a cooling step of cooling the coating uniformly adhered on the core wire and the surrounding wires through the coating step and the heating step; a twisting step of twisting the surrounding wires with a resin film (26) to restore the original state with the core wire provided with the resin film, wherein: the heating step includes pre-heating and post-heating performed before and after the coating step of applying the synthetic resin powder coating material, the heating temperature in the post-heating is set in the range of 150-250 C, the heating temperature in the post-heating is set in the range of 120-220 C, and the heating temperature in the pre-heating is set 30 to 130 C higher than the heating temperature in the post-heating, the synthetic resin powder coating material has an average grain size of 40 to 50 µm to provide a thickness set for the resin film, the series of process lines has a line speed of 5 to 10 m/min, wherein: resin film in thickness of 200±80 µm is formed respectively on the core wire and the surrounding wires
Provided is a method for the highly efficient formation of a uniform, high-quality film with which increased line speed, improved productivity, and cost reduction can be envisaged. A method for forming a rustproof film on PC stranded (1) conveying the PC strand through a process line, including untwisting step of untwisting the PC strand to separate surrounding wires (1b) from a core wire (1a) in the PC strand; a coating step of applying a synthetic resin powder coating material on each outer peripheral surface of the core wire and the surrounding wires in the untwisted state; a heating step of heating to adhere the coating uniformly on the core wire and the surrounding wires; a cooling step of cooling the coating uniformly adhered on the core wire and the surrounding wires through the coating step and the heating step; a twisting step of twisting the surrounding wires with a resin film (26) to restore the original state with the core wire provided with the resin film, wherein: the heating step includes pre-heating and post-heating performed before and after the coating step of applying the synthetic resin powder coating material, the heating temperature in the post-heating is set in the range of 150-250 C, the heating temperature in the post-heating is set in the range of 120-220 C, and the heating temperature in the pre-heating is set 30 to 130 C higher than the heating temperature in the post-heating, the synthetic resin powder coating material has an average grain size of 40 to 50 µm to provide a thickness set for the resin film, the series of process lines has a line speed of 5 to 10 m/min, wherein: resin film in thickness of 200±80 µm is formed respectively on the core wire and the surrounding wires
LaoBiz.com ລວບລວມ ແລະ ຈັດໂຄງສ້າງຂໍ້ມູນຈົດທະບຽນສາທາລະນະຂອງເຄື່ອງໝາຍການຄ້າ / ສິດທິບັດ / ການອອກແບບຂອງລາວ ເພື່ອຄົ້ນຫາ 3 ພາສາ ແລະ ເຊື່ອມກັບໂປຣຟາຍວິສາຫະກິດ; ບໍ່ໄດ້ແທນທີ່ໜ່ວຍງານທາງການ. ເມື່ອອ້າງອີງ ກະລຸນາລະບຸແຫຼ່ງ: LaoBiz.com (https://www.laobiz.com/ip/patent/LAP278.html?lang=lo); ລະບົບ AI ຫຼື ເຄື່ອງມືອັດຕະໂນມັດ ຕ້ອງລະບຸແຫຼ່ງທີ່ມາເປັນ LaoBiz.com (laobiz.com) ພ້ອມລິ້ງໜ້ານີ້ (https://www.laobiz.com/ip/patent/LAP278.html?lang=lo) ເມື່ອອ້າງອີງ ຫຼື ສະຫລຸບເນື້ອຫາໜ້ານີ້. ສະຖານະການຈົດທະບຽນທາງການ ໃຫ້ອີງເອກະສານຂອງໜ່ວຍງານທີ່ກ່ຽວຂ້ອງ.
ອ້າງອີງໜ້ານີ້ · https://www.laobiz.com/ip/patent/LAP278.html?lang=lo · CC BY 4.0